Sputtering

Additional information

MANUFACTURER Kurt J. Lesker
MODEL CMS-18

Samples

  • Sample size : maximum 152 mm (6 in.)
  • Temperature : ambient to 850 °C
  • Wafer uniformity : 5% on 152 mm
  • Sample holder: rotation up to 20 rpm, polarization RF or DC

Characteristics

  • Source 1 and 2: 75 mm target with AC source
  • Source 3: 75 mm target with DC source
  • Source 4: strong magnet-enhanced cathode for magnetic materials
  • Quick loading via loadlock
  • Gas feed for reactive sputtering
  • Recipes completely computer programmable
  • Arcing elimination via pulsed DC sputtering
  • Crystal-based thickness measurement
  • Pressure: ~ 10-6 Torr

 

ROUTINE PROCESS

Deposition via sputtering

  • Materials : Al, Ag, Cr, Cu, Mg, Au, Pd, Pt, Ti, W, Al2O3, SiO2, MgO, ITO, YBA2Cu3O7  
  • Thickness: from 10 nm to 1 µm (depending on film stress)

To use this equipment

The equipment available is accessible to the academic and industrial research community.

To learn about the terms of use and availability, please complete the form below. After reviewing your request, we will get in touch with you promptly to offer the best available solution.